  • 摘要: 针对水电站泄洪闸自润滑关节轴承在重载、小角度往复摆动条件下主承载区易发生局部磨损的问题,建立有限元接触模型,选取5 000、6 500和8 000 kN三种载荷工况,分析0~0.5 mm磨损过程中外圈内球面接触应力演化规律。基于Archard磨损模型,按接触应力相对分布更新磨损型线,并结合文献寿命数据得到的应力相关等效磨损系数计算摆动次数。结果表明,无磨损状态下,载荷由5 000 kN增至8 000 kN时,最大接触应力由163.43 MPa增至259.46 MPa;磨损至0.5 mm时,三种载荷下最大接触应力分别为271.02、312.28和355.23 MPa,累计摆动次数分别为81 675、18 637和5 615次。载荷升高与磨损累积共同加剧主承载区应力集中,并加速磨损寿命衰减。研究结果可为泄洪闸自润滑关节轴承磨损寿命评估和载荷控制提供参考。

     

    Abstract: To investigate the localized wear of self-lubricating spherical plain bearings used in hydropower spillway gates under heavy-load and small-amplitude oscillatory motion, a finite element contact model was established, and three load cases of 5 000, 6 500, and 8 000 kN were selected to analyze the evolution of contact stress on the inner spherical surface of the outer ring over a wear-depth range of 0-0.5 mm. Based on the Archard wear model, the worn surface profile was iteratively updated according to the relative distribution of contact stress, and the number of oscillation cycles was evaluated using a stress-dependent equivalent wear coefficient derived from service-life data reported in the literature. The results indicate that, in the unworn state, the maximum contact stress increases from 163.43 MPa to 259.46 MPa as the applied load rises from 5 000 to 8 000 kN. At a wear depth of 0.5 mm, the maximum contact stresses under loads of 5,000, 6,500, and 8 000 kN reach 271.02, 312.28, and 355.23 MPa, respectively, and the corresponding cumulative oscillation cycle numbers are 81 675, 18 637, and 5 615. Increasing load and accumulated wear jointly intensify stress concentration in the primary load-bearing region, thereby accelerating wear progression and shortening oscillation life. The results provide a reference for wear-life assessment and load-control strategies for self-lubricating spherical plain bearings used in hydropower spillway gates.

     

/

返回文章
返回