  • 摘要: 针对TiAl4822合金室温塑性差及耐磨、耐腐蚀性能有待提升等问题,采用选择性激光熔化(selective laser melting,SLM)技术制备TiAl4822/TiC合金,系统研究了激光功率(100~160 W)和扫描速度(800~1 200 mm/s)对合金摩擦学及电化学腐蚀性能的影响。研究结果表明,SLM成形TiAl4822/TiC合金的主要物相为Ti-Al基金属间化合物,其中Ti0.6Al0.4为主要相。不同工艺参数下试样显微硬度介于385~477 HV,其中在160 W、1000 mm/s条件下获得最高显微硬度。摩擦学测试结果表明,合理的工艺参数能够有效提高合金耐磨性能,其中在160 W、1 200 mm/s的参数组合下,试样表现出最优的综合耐磨性能,其磨损体积仅为0.019 mm3。工艺参数为140 W、1 000 mm/s的试样具有最优的耐腐蚀性能,其腐蚀电位为−361.26 mV,而腐蚀电流密度显著降低至最小值3.36×10−7 A/cm2。本研究可为SLM制备高性能TiAl4822/TiC合金的工艺优化及工程应用提供实验依据和理论参考。

     

    Abstract: In response to the problems of poor room-temperature plasticity and the need for improvement in wear resistance and corrosion resistance of the TiAl4822 alloy, the TiAl4822/TiC alloy was fabricated using selective laser melting (SLM) technology. The effects of laser power (100-160 W) and scanning speed (800-1200 mm/s) on the frictional and electrochemical corrosion properties of the alloy were systematically investigated. The results showed that the main phase of the SLM-formed TiAl4822/TiC alloy was Ti-Al-based intermetallic compounds, with Ti0.6Al0.4 being the main phase. The microhardness of the samples varied between 385-477 HV, with the highest microhardness achieved under the conditions of 160 W and 1000 mm/s. The frictional test results indicated that reasonable process parameters could effectively improve the wear resistance of the alloy. Under the parameter combination of 160 W and 1200 mm/s, the sample exhibited the best comprehensive wear resistance, with a wear volume of only 0.019 mm3. The sample with process parameters of 140 W and 1000 mm/s had the best corrosion resistance, with a corrosion potential of −361.26 mV and a corrosion current density significantly reduced to the minimum value of 3.36×10−7 A/cm2. This study can provide an experimental basis and theoretical reference for the process optimization and engineering application of SLM in the preparation of high-performance TiAl4822/TiC alloy.

     

/

返回文章
返回